| Sign In | Join Free | My rc363.com |
|
Brand Name : JINHAIHU
Model Number : DSC-1150B
Certification : ISO
Place of Origin : BEIJING, CHINA
MOQ : 1 set
Payment Terms : T/T,L/C,Western Union,MoneyGram,D/A,D/P
Supply Ability : 20 sets per month
Delivery Time : 7-15 working days
Packaging Details : Conventional export wooden crates
Product name : Calorimeter DSC Plastic Differential Scanning Calorimetry Price
Model : DSC-1150B
DSC range : 0~±500 mw
Temperature range : RT ~1150℃
Aluminum crucibles : Φ6.6*3mm (Diameter * High)
Ceramic crucibles : Φ6.6*3mm (Diameter*High)
Customized support : OEM, ODM
Melting and crystallization temperature and enthalpy measuring instrument
Application:
DSC is designed for determining internal heat transitions related to temperature and heat flow, widely applied in polymer development, performance testing, and quality control. DSC research and development covers the following fields: glass transition temperature, melting point, cold crystallization, crystallization, phase transition, and oxidation induction time (OIT).
The instrument features:
1.LCD liquid crystal display with blue backlight, showing comprehensive information: set temperature, sample temperature, oxygen flow, nitrogen flow, differential thermal signal, and various switch statuses.
2.USB communication interface for data transfer.
3.Compact furnace body design with infinitely adjustable temperature rise rate.
4.Dual temperature probes ensure repeatable sample temperature measurement at specified heights.
5.Digital gas mass flow meter enables automatic switching of two-way atmosphere flow, featuring fast response and short stabilization time.
6.Calibrated with standard samples for easy customer adjustment of the constant temperature coefficient.
7.Furnace cooling interface for rapid temperature reduction as needed.
8.Software compatible with laptops and desktops, supporting Win2000, XP, VISTA, WIN7 and other operating systems.
9.Supports user-defined programming to automate measurement procedures.


| Temperature range | RT-1150℃ |
| Temperature resolution | 0.01℃ |
| Heating rate | 0.1~80℃/min |
| Constant temperature | RT-1150℃ |
| Duration of constant temperature | The constant temperature time is unlimited at low temperature; When more than 1000 ℃, it is recommended that a single constant temperature time is less than 30 min |
| Temperature control mode | Heating, cooling, constant temperature, any combination of three modes cycle use, temperature uninterrupted |
| DSC range | 0~±500mW |
| DSC resolution | 0.01mW |
| DSC sensitivity | 0.01mW |
| Working power | AC 220V 50Hz 300W or other |
| Atmosphere control gas | Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen) |
| Gas flow | 0-200mL/min |
| Gas pressure | 0.2MPa |
| Gas flow accuracy | 0.2mL/min |
| Crucible | Aluminium crucible Φ6.6*3mm (Diameter * High),ceramic crucible Φ6.6*3mm (Diameter * High) |
| Calibration standard | With standard material (Indium, tin, zinc, silver), users can adjust the temperature coefficient and enthalpy value coefficient by themselves |
| Data interface | Standard USB interface |
| Display mode | 7-inch touch screen |
| Output mode | computer and printer |
| Design features | Fully closed support structure design, prevent items falling into the furnace body, pollution of the furnace body, reduce the maintenance rate |




|
|
Plastic DSC Differential Scanning Calorimetry 500mw For Glass Transition Temperature Images |